Physical Properties | ||||
Properties | Unit | Values | Test standard | |
Basic | Density | g/cm3 | 1.19 | ISO 1183 |
Transmittance | % | 92 | DIN 5036 | |
Water absorption | mg | 41 | ISO62,Method 1 | |
Weather resistant | -- | excellent | -- | |
Mechanical | Tensile strength | Mpa | 80 | ISD 527-2/1B/5 |
Flexural strength | Mpa | 115 | ISO 178 | |
Modulus of elasticity | Mpa | 3300 | ISD 527-2/1B/1 | |
Izod Notched impact strength(Lzod) | Kj/m2 | 1.6 | ISO 180/1A | |
Charpy Notched impact strength(Charpy) | Kj/m2 | 15 | ISO 179/1fu | |
Elongationat break | % | 5.5 | ISO 527-2/1B/5 | |
H961/30 Indentation hardness H961/30 | Mpa | 175 | ISO 2039-1 | |
Thermal | Forming temperature | ℃ | 160-175 | -- |
Heat deflection temperature | ℃ | 115 | ISO 75 | |
Max.permanent service temperature | ℃ | 80 | -- | |
Coefficient of linear thermal expansion | 1/K | 7x10-5 | DIN 53752-A | |
Electrical | Volume resistivity | Ω.cm | >1015 | DIN VDE 0303 |
Surface resistivity | Ω | 5x1013 | DIN VDE 0303 | |
Dielectric strength | KV/mm | 30 | DIN VDE 0303 |